MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® PF004EUC PA6-GF20
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Vydyne PF004EUC is a 20% glass fiber reinforced PA6 for injection molded applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccDAM; ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPaDAM; ISO 527-2
Tensile Strength, Yield 117 MPaDAM; ISO 527-2
Elongation at Yield 3.0 %DAM; ISO 527-2
Tensile Modulus 6300 MPaDAM; ISO 527-2
Flexural Strength 163 MPaDAM; ISO 178
Flexural Modulus 4800 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 500 V
@Thickness 3.00 mm
IEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 177 °CUnannealed; DAM; ISO 75-2/A
Glow Wire Flammability Index 650 °C
@Thickness 1.60 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 230 - 240 °CInjection
Middle Barrel Temperature 240 - 250 °CInjection
Front Barrel Temperature 240 - 270 °CInjection
Melt Temperature 240 - 270 °CInjection
Mold Temperature 60.0 - 80.0 °CInjection
Drying Temperature 75.0 - 85.0 °CInjection
Dry Time 4.00 hourInjection
Moisture Content 0.20 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Release agent
Agency RatingsISO, 1043 PA6 GF20
AppearanceNatural Color
FeaturesGood Stiffness
 Good Strength
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE8527 / 296330

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.