(Viewing data as-entered.
Click here
to return)
Ashley Polymers Ashlene® 68MG Nylon 66, Glass/Mineral reinforced
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Glass/Mineral Filled
Material Notes:
A glass/mineral reinforced nylon offering excellent dimensional stability and rigidity.
Data provided by the manufacturer
Key Words:
Polyamide 66; Ashley Polymers, Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.44
g/cc
ASTM D792
Mechanical Properties
Original Value
Comments
Tensile Strength, Ultimate
131
MPa
ATSM D638
Elongation at Break
5.0 %
ASTM D638
Flexural Modulus
6.90
GPa
ASTM D790
Izod Impact, Notched
0.530
J/cm
ASTM D256
Thermal Properties
Original Value
Comments
Melting Point
254
°C
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi)
241
°C
ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Envalior EcoPaXX® Q-HG6 PA410-GF30
RTP Company RTP 2099 X 121249 C Bio-Based Polylactic Acid (PLA); Standard Nucleator - Glass Fiber - 68% Renewable Resource Content
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
Overview of materials for Nylon 46, Glass Fiber Reinforced
Envalior EcoPaXX® Q-X07209 PA410-I-GF40
PNAB06 / 54453
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.