MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayflex® 953 Polyether-based Polyurethane System, Density 34 pcf
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Bayflex 953 is a fully compounded polyether-based polyurethane system consisting of two liquid components which can be water-blown.

Properties / Applications: Bayflex 953 is a fully compounded polyether-based polyurethane system consisting of two liquid components which can be water-blown. Component A is a modified diphenylmethane diisocyanate (MDI) prepolymer, and Component B is a polyether polyol system. The Bayflex 953 system is used in the manufacture of microcellular polyurethane shoe soles. Soles prepared from these components combine light weight, comfort, and durability. Processibility and dynamic flexural properties are excellent over a wide range of densities. The combination of excellent physical properties and ease of processing has made the Bayflex 953 system a prime material for single-density soles for fashion and casual shoes. As with any product, use of the Bayflex 953 system in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.520 g/ccMolded
 1.06 g/ccPolyol (Component B)
 1.20 g/ccIsocyanate (Component A)
Viscosity 1100 cPIsocyanate (Component A)
 1100 cPPolyol (Component B)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50ASTM D2240
Tensile Strength at Break 3.10 MPaASTM D412
Elongation at Break 400 %ASTM D412
Tear Strength 25.0 pliBlack
 80.0 pliDie C; ASTM D1004
Taber Abrasion, mg/1000 Cycles 70
@Load 1.00 kg
H-18; ASTM D4060
 
Thermal PropertiesOriginal ValueComments
Flash Point 132 °CPolyol (Component B)
 207 °CIsocyanate (Component A)
 
Processing PropertiesOriginal ValueComments
Mold Temperature 49.0 °C
Moisture Content <= 0.46 %Polyol (Component B)
 
Descriptive Properties
AppearanceLight yellow viscous liquidIsocyanate (Component A)
 Milky white liquidPolyol (Component B)
Content18.7-19.1%NCO, Isocyanate (Component A)
Hydroxyl numberPolyol (Component B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayflex® 970 Polyether-based Polyurethane System, Density 34 pcf
Lubrizol Advanced Materials Pearlthane® Clear 15N70 Polyether based TPU
Covestro Bayflex® 952 Polyether-based Polyurethane System, Density 34 pcf
Covestro Bayflex® 906 Polyether-based Polyurethane System, Density 34 pcf
Covestro Bayflex® 906 Polyether-based Polyurethane System, Density 29 pcf

PCOVEST0129 / 201912

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.