MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CIMBAR RP 9405 Talc
Categories: Ceramic; Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: RP 9400 Series talcs are produced from ores, which provide an excellent balance of mechanical properties at an economical price, for primary use in commodity polypropylene. RP 9400 Series talcs are platy, hydrophobic, non-abrasive and chemically inert.
9400 Series talcs industrial applications include: thermoplastics, thermosets, adhesives & mastics and rubber dusting.

Information provided by Cimbar Performance Minerals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.78 g/cc
Bulk Density 24.0 lb/ft³Loose
 68.0 lb/ft³Tapped
Brightness 85 %Hunter Rd, dry
Oil Absorption 26 %g oil/100 g filler; ASTM D281
Moisture Absorption at Equilibrium 0.30 %
Loss On Ignition 17 %
Particle Size 5.0 µm@ 10%
 6.5 µmD50
 26 µm@ 98%
Particle Mesh Size 325 Mesh0.2% retained
pH 9.2
 
Component Elements PropertiesOriginal ValueComments
Al2O3 <= 1.0 %
CaO <= 14 %
Fe2O3 <= 1.0 %
MgO 24 %
SiO2 46 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CIMBAR EliteTalc® 20 Cosmetic Talc
CIMBAR RP 9305 Talc
CIMBAR RP 9410 Talc
CIMBAR EliteTalc® 22 Cosmetic Talc
CIMBAR EliteTalc® 23 Cosmetic Talc

CIMBAR931 / 133413

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.