MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
General Plastics LAST-A-FOAM® FR-6720 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Product Description: LAST-A-FOAM® FR-6700 is a CFC-free, rigid, closed-cell, flame-retardant polyurethane foam for aircraft composite core that withstands process temperatures up to 250°F. It is available in densities ranging from 10 to 25 pounds per cubic foot and exhibits a high strength-to-weight ratio due to its cellular structure and cross-linked resin. Because of its closed-cell structure, LAST-A-FOAM® FR-6700 has great resistance to water absorption and will not swell, crack, or split on exposure to water.

Product Feature:

  • Stable
  • Inert
  • Will not support fungal growth
  • Resistant to most chemicals and solvents
  • Easily shaped with common woodworking tools
  • Performs well as wood replacement
Applications:
  • Models and design prototypes
  • Composite Core
  • Honeycomb edge close-out for aircraft interior sandwich panels used in overhead storage bins, passenger cabin class dividers, galleys and lavatories
  • Vacuum form dies and mold patterns

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 g/ccASTM D1622
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 35.6cut foam surface; ASTM D2240
Tensile Strength 793 psiPerpendicular to Rise; ASTM D1623
 801 psiParallel to Rise; ASTM D1623
Flexural Strength 1224 psiRise Parallel to Beam Thick.; ASTM D790
 1226 psiRise Parallel to Test Span; ASTM D790
Flexural Modulus 42373 psiRise Parallel to Test Span; ASTM D790
 43349 psiRise Parallel to Beam Thick.; ASTM D790
Compressive Strength 508 psi
@Temperature 121 °C
Parallel to Rise; ASTM D1621
 544 psi
@Temperature 121 °C
Perpendicular to Rise; ASTM D1621
 801 psi
@Temperature 93.3 °C
Parallel to Rise; ASTM D1621
 805 psi
@Temperature 93.3 °C
Perpendicular to Rise; ASTM D1621
 1392 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 1398 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
 2136 psi
@Temperature -53.9 °C
Perpendicular to Rise; ASTM D1621
 2151 psi
@Temperature -53.9 °C
Parallel to Rise; ASTM D1621
Compressive Modulus 17416 psi
@Temperature 121 °C
Parallel to Rise; ASTM D1621
 17417 psi
@Temperature 121 °C
Perpendicular to Rise; ASTM D1621
 24922 psi
@Temperature 93.3 °C
Parallel to Rise; ASTM D1621
 25102 psi
@Temperature 93.3 °C
Perpendicular to Rise; ASTM D1621
 35401 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 36759 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
 40229 psi
@Temperature -53.9 °C
Perpendicular to Rise; ASTM D1621
 40832 psi
@Temperature -53.9 °C
Parallel to Rise; ASTM D1621
Poissons Ratio 0.30
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µin/in-°F
@Temperature 23.9 - 121 °C
 350 µin/in-°F
@Temperature -45.6 - 93.3 °C
GP Method
Specific Heat Capacity 0.376 BTU/lb-°FASTM E1269
Thermal Conductivity 0.405 BTU-in/hr-ft²-°FASTM C518
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -320 °F
Glass Transition Temp, Tg 275 °FASTM E1824
 
Descriptive Properties
Closed Cell Content68%25 lbs/ft3
 96%10 lbs/ft3
Heat of Combustion10939 BTU/lbASTM D240
Tumbling Friability (%)125 lbs/ft3
 10.8910 lbs/ft3
Water Absorption0.01 lbs/ft²18 lbs/ft³
 0.049 lbs/ft²10 lbs/ft³

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® FR-6718 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3703 Polyurethane Foam
BCC Products MB 1200 Polyurethane Foam Modeling Board
Covestro Baynat® 3002 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3706 Polyurethane Foam

PGENR040 / 186826

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.