MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Arlon 56224R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
Side 1: Uncured Silicone Rubber

This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 76.2 microns3.00 milPolyethylene, Interleave
 >= 203 microns>= 8.00 milSide 1
 432 microns17.0 milPrime Coated 1564 Fiberglass, Substrate
 584 - 686 microns23.0 - 27.0 milOverall
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55 - 6055 - 60Compound Property
Tensile Strength >= 6.21 MPa>= 900 psiCompound Property
Elongation at Break >= 200 %>= 200 %Compound Property
Peel Strength >= 0.877 kN/m>= 5.00 pliBond Strength
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 15.7 kV/mm>= 400 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 177 °C
0.250 hour
@Temperature 350 °F
Recommended Cure Cycle
 120 min
@Temperature 232 °C
2.00 hour
@Temperature 450 °F
Recommended Postcure Cycle
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
From date of manufacture
 
Descriptive Properties
ColorRed
Total Product Weight (oz/yd2)31.2 - 37.2
Uncoated Fabric Break Strength350 lb/inFill Direction, Substrate Property
 400 lb/inWarp Direction, Substrate Property

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARL413 / 125599

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.