MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NRI Solar-Wrap Fiberglass wrap
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Description: Solar-Wrap™ is a pre-impregnated, bi-directional fiberglass wrap utilizing a UV-curable polyester based resin system. It has been designed to be a very fast return-to-service product which can be applied at any temperature without extended curing times. This has been achieved by using a curing process that utilizes UV light and is relatively independent of temperature. Solar Wrap is provided as a roll of pre-impregnated, woven fiberglass tape in a UV-stable foil pouch and should not be removed outdoors without proper UV cover. Solar Wrap is an excellent and versatile solution for any industry where quick-action repair in adverse conditions is a critical aspect for successful operations.

Typical Applications:

  • Emergency repair
  • Corroded pipes
  • Irregular pipe fittings
  • Force mains and gravity lines
  • Joint, tee, and elbow repair
Benefits:
  • Controlled curing process
  • Application in low temperature environment without extend cure time
  • UV stable
  • No field mixing or impregnating required
  • Effectively seals out atmospheric conditions, preventing future corrosion

Information provided by NRI® Innovative Composite Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 61 - 65 %
Thickness 13.0 milper ply
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72ASTM D2240
Tensile Strength 433 MPaASTM D3039
Tensile Modulus 19.7 GPaASTM D3039
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 56.0 °C
Heat Distortion Temperature 71.0 °CASTM D648
Minimum Service Temperature, Air -46.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 - 5.00 minStrong UV
 5.00 - 6.00 minMedium UV
 6.00 - 9.00 minLow UV
Shelf Life 4.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Isoflon Tisoflon® 3 AD Polytetrafluoroethylene Coated Glass Fabric
Isoflon Tisoflon® 6 AD EXTRA SMOOTH Polytetrafluoroethylene Coated Glass Fabric
NRI Syntho-Glass® 24 Fiberglass Mat
Isoflon Tisoflon® 10 AD Polytetrafluoroethylene Coated Glass Fabric
Isoflon Tisoflon® 5 AD Polytetrafluoroethylene Coated Glass Fabric

PNRI012 / 192028

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.