MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teijin Panlite® LN-2250Y Flame Resistant, Translucent Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Flame retardant and mold release grade with normal fluidity, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications.

Applications:

  • Electric, electronic and business machine components that need flame retardancy.
  • Information provided by Teijin Chemicals Ltd.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.20 g/ccISO 1183
    Moisture Absorption 0.200 %
    @Temperature 23.0 °C,
    Time 86400 sec
    ISO 62
    Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
    @Thickness 4.00 mm
    Teijin method
    Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
    @Thickness 4.00 mm
    Teijin method
    Melt Flow 13.2 g/10 min
    @Load 1.20 kg,
    Temperature 300 °C
    ISO 1133
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength, Yield 61.0 MPaISO 527-2/50
    Elongation at Break >= 50 %ISO 527-2/50
    Elongation at Yield 6.0 %ISO 527-2/50
    Tensile Modulus 2400 MPaISO 527-2/1
    Flexural Strength 92.0 MPa2.0 mm/min; ISO 178
    Flexural Modulus 2350 MPa2.0 mm/min; ISO 178
    Charpy Impact Unnotched NBISO 179
    Charpy Impact, Notched 76.0 kJ/m²ISO 179
     
    Electrical PropertiesOriginal ValueComments
    Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
    Surface Resistance >= 1.00e+15 ohmIEC 60093
    Dielectric Constant 3.0
    @Frequency 1e+6 Hz
    IEC 60250
     3.1
    @Frequency 100 Hz
    IEC 60250
    Dielectric Strength 32.0 kV/mmshort time test; IEC 60243-1
    Dissipation Factor 0.0010
    @Frequency 100 Hz
    IEC 60250
     0.0090
    @Frequency 1e+6 Hz
    IEC 60250
    Comparative Tracking Index 225 VIEC 60112
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear, Parallel to Flow 70.0 µm/m-°CISO 11359-2
    CTE, linear, Transverse to Flow 70.0 µm/m-°CISO 11359-2
    Deflection Temperature at 0.46 MPa (66 psi) 141 °Cunannealed; ISO 75-2/B
    Deflection Temperature at 1.8 MPa (264 psi) 128 °Cunannealed; ISO 75-2/A
    Vicat Softening Point 148 °CISO 306/B50
    UL RTI, Electrical 125 °C
    @Thickness 3.00 mm
    UL 746
    UL RTI, Mechanical with Impact 115 °C
    @Thickness 3.00 mm
    UL 746
    UL RTI, Mechanical without Impact 125 °C
    @Thickness 3.00 mm
    UL 746
    Flammability, UL94 V-2
    @Thickness 0.430 mm
     V-0
    @Thickness 3.00 mm
    Glow Wire Ignition Temperature 850 °C
    @Thickness 1.00 mm
    IEC 60695-2-13
     850 °C
    @Thickness 3.00 mm
    IEC 60695-2-13
    Glow Wire Flammability Index 900 °C
    @Thickness 1.00 mm
    IEC 60695-2-12
     960 °C
    @Thickness 3.00 mm
    IEC 60695-2-12
     
    Optical PropertiesOriginal ValueComments
    Refractive Index 1.585ASTM D-542
    Transmission, Visible 88 %
    @Thickness 3.00 mm
    ASTM D-1003

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Teijin Panlite® K-1300Y Standard (mold release/ice color grade) Polycarbonate Resin
    Teijin Multilon TN-7500 Halogen-Free Flame Resistant PC/ABS Polymer Alloy
    Teijin Multilon TN-7100F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
    Teijin Panlite® L-1225Z100 Weather Resistant Grade Polycarbonate
    Teijin Multilon T-3011 Standard PC/ABS Polymer Alloy

    PTEIJ14 / 69703

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.