MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Precision Polymer Engineering Perlast® G75B High Temperature Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Perlast® G75B offers a unique blend of excellent chemical resistance, temperature capabilities and mechanical properties, simultaneously extending the operating limits in all three aspects. Perlast® G75B has been specially formulated to provide increased acid resistance by eliminating fillers that are prone to acid attack and optimising the polymer structure. In addition, this perfluoroelastomer has low permeability and as a result, it is less prone to swelling, leading to extended in-service performance in, for example, valves, pumps and mechanical seals. A high modulus makes G75B resistant to extrusion and ideal for use in high pressure environments. In addition, the low long-term compression set provides a high mean-time between maintenance cycles in hot chemically aggressive environments. Perlast® G75B is suitable for both dynamic and static applications and can be moulded into O-rings and custom shapes.

Applications: Aerospace: Inter-stage seal assemblies (static O-rings). Chemical Processing: Pumps; Valves; Mechanical seals. Diesel: Cylinder bore liners (static O-rings); Exhaust valve seats. Semiconductor: Gas abatement systems (static); High vibration environments. Oil & Gas: High temperature down-hole environments; Electrical bulkhead feed-throughs.

Key Words: Rubbers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 78ASTM D1415
 79ASTM D2240
Tensile Strength, Yield 19.2 MPaASTM D412
Elongation at Break 131 %ASTM D412
100% Modulus 0.0120 GPa
@Strain 100 %
ASTM D412
Compression Set 26 %
@Temperature 200 °C,
Time 259000 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
CTE, linear 400 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 325 °C
Minimum Service Temperature, Air -15.0 °C
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Precision Polymer Engineering Perlast® G80A Perfluoroelastomer
Precision Polymer Engineering N90M Nitrile Rubber
Precision Polymer Engineering E70Q Ethylene Propylene Rubber
Freudenberg Simriz® 483 Low Temperature FFKT Perfluoroelastomer Compound
Precision Polymer Engineering Perlast® G80T Perfluoroelastomer

PPRECI024 / 57748

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.