MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Durethan® AKV 30 HR H2.0 900116 Nylon 66, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183
Water Absorption 5.5 %Test Sim. to ISO 62
Moisture Absorption at Equilibrium 2.0 %23°C/50% R.H.; Test Sim. to ISO 62
Melt Flow 14 g/10 min
@Load 5.00 kg,
Temperature 280 °C
Estimated using room temperature density; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 120 MPaConditioned; ISO 527-1/-2
 180 MPaISO 527-1/-2
Elongation at Break 4.0 %ISO 527-1/-2
 8.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 6100 MPaConditioned; ISO 527-1/-2
 9500 MPaISO 527-1/-2
Charpy Impact Unnotched 75.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 75.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 85.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 90.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 <= 10.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 20.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned; IEC 60093
 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
IEC 60250
 4.5
@Frequency 1e+6 Hz
Conditioned; IEC 60250
 12
@Frequency 100 Hz
Conditioned; IEC 60250
Dielectric Strength 30.0 kV/mmConditioned; IEC 60243-1
 35.0 kV/mmIEC 60243-1
Dissipation Factor 0.0080
@Frequency 100 Hz
IEC 60250
 0.016
@Frequency 1e+6 Hz
IEC 60250
 0.090
@Frequency 1e+6 Hz
Conditioned; IEC 60250
 0.30
@Frequency 100 Hz
Conditioned; IEC 60250
Comparative Tracking Index 450 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°CISO 11359-1/-2
Melting Point 263 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 250 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 245 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 125 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 HB
@Thickness 3.20 mm
IEC 60695-11-10
Oxygen Index 25 %ISO 4589-1/-2
 
Descriptive Properties
FormPellets
ISO Short NameISO 1874-PA 66,MHWR,18-100,GF30
ProcessingInjection molding
RegionAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber
Lanxess Durethan® AKV 30 H1.0 000000 Nylon 66, 30% Glass Fiber
Domo TECHNYL® R AR 218 V30 Nylon 66, 30% glass fiber, DRY
Celanese Zytel® 70G30HSLR BK099 PA66-GF30
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced

PLANX0712 / 98927

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.