MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Seals Eastern 7075 Ethylene-Propylene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: General service EPDM.

Information provided by Seals Eastern, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D297, 15
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 62>= 62ASTM D2240, Type A
 7373AVG; ASTM D2240, Type A
Tensile Strength at Break >= 10.31 MPa>= 1496 psiASTM D412 Method A
 20.3 MPa2940 psiAVG; ASTM D412 Method A
Tensile Stress at Strain  >= 1.31 MPa
@Strain 50 %
>= 190 psi
@Strain 50 %
Minimum; ASTM D412 Method A
 1.45 MPa
@Strain 25 %
210 psi
@Strain 25 %
Average; ASTM D412 Method A
 >= 2.00 MPa
@Strain 100 %
>= 290 psi
@Strain 100 %
Minimum; ASTM D412 Method A
 2.14 MPa
@Strain 50 %
310 psi
@Strain 50 %
Average; ASTM D412 Method A
 3.93 MPa
@Strain 100 %
570 psi
@Strain 100 %
Average; ASTM D412 Method A
Elongation at Break >= 205 %>= 205 %ASTM D412 Method A
 410 %410 %AVG; ASTM D412 Method A
Modulus of Elasticity 0.00993 GPa1.44 ksiASTM D412 Method A
Poissons Ratio 0.500.50Calculated
Shear Modulus 0.00331 GPa0.480 ksiASTM D412 Method A
Secant Modulus 0.009329 GPa1.353 ksiASTM D412 Method A
Tear Strength Test 134134(psi); ASTM D624, Die B
Compression Set 13 %
@Temperature 100 °C,
Time 79200 sec
13 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395, Test B
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -51.1 °C-60.0 °FASTM D1329
 
Descriptive Properties
Strain Energy / Unit Volume at 20% Elongation (psi)26

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Seals Eastern 7045 Ethylene-Propylene Rubber
Seals Eastern 7267 Ethylene-Propylene Rubber
Alclad Aluminum 7075-O
Seals Eastern 5053 Ethylene-Propylene Rubber
Seals Eastern 7189 Ethylene-Propylene Rubber

PSEAL25 / 80172

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.