MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mueller Ecostream™ GreenDrop™ C27451 DZR Lead Free Plumbing Brass
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Mueller Brass Company has developed a dezincification resistant version of its GreenDrop™ C27450 Lead Free Brass Alloy. This new alloy, C27451, is specifically designed for machined or forged parts and components requiring compliance to both lead free and dezincification resistance criteria adopted by potable water and PEX standards and applications.
Compliant • Competitive • Compatable
Although specifically developed for parts requiring compliance to dezincification resistance standards; Mueller Brass Company’s C27451 alloy still retains the same inherent advantages over other lead free alloys offered by other manufacturers. With the customer as its core focus, Mueller Brass Company developed C27451 to not only aide manufacturers with their compliance needs, but also develop an alloy that would help manufacturers control their material costs and retain their competitive advantage. Since no expensive additives or potential contaminants like silicon or bismuth are added, C27451 DZR Lead Free Brass is completely recyclable and compatible with all EcoStream™ and conventional leaded alloys widely used today. Since the need for segregation, the cleaning out of machines or the rejection of contaminated scrap is virtually eliminated; C27451 offers the manufacturer the additional benefits of manufacturing efficiency and productivity.

Advantanges:

  • Good machinability
  • Excellent forgeability
  • Excellent brazing and plating
  • Excellent ability to Thread Roll
  • Dezincification Resistant

Applications:

  • Potable water components, fixtures and applications
  • PEX plumbing applications and systems
  • Forged products requiring lead free and/or dezincification compliance

Information Provided by Mueller Industries Inc.

Key Words: UNS C27451
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 55 - 75
Tensile Strength at Break 55000 psi
Tensile Strength, Yield 35000 psi
Elongation at Break 30 %
Machinability 70 %
Forgeability 95 %
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 60 - 65 %
Iron, Fe <= 0.35 %
Lead, Pb <= 0.25 %
Other <= 0.50 %
Phosphorus, P 0.050 - 0.12 %
Zinc, Zn 33.78 - 39.95 %Remainder
 
Descriptive Properties
BrazingExcellent
Cold WorkingExcellent
PlatingExcellent
SolderingExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Free-cutting phosphor bronze, UNS C54400, H04 Temper 25 mm rod
Herculoy®, High-Silicon Bronze A, UNS C65500, H04 Temper flat products
Dezincification Brass, DZR, UNS C35330
316 Stainless Steel, annealed and cold drawn bar
304 Stainless Steel

NMUEL904a / 140850

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.