MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Honeywell PTM1300-SP
Categories: Polymer

Material Notes: PTM1300-SP is a highly compressible thermal interface material developed for applications in the memory and mobile electronics markets. It provides stable performance in low pressure environments, allowing manufacturers a wider process window in thermal module assembly. PTM1300-SP offers the same quality and reliability as Honeywell’s other industry-leading phase change materials. PTM1300-SP has an optimized filler size distribution to achieve maximum packing density compared to conventional phase change materials. PTM1300-SP changes phase at 45°C to ensure maximum surface conformance, and may be applied to a component, heat sink or thermal spreader.

Features & benefits:

  • Wider process window in module assembly
  • Stable thermal performance, even after thermal cycling and HAST
  • Provides excellent compliance and rapid thermal response
  • Simple to apply
  • Superior handling and reworkability

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 g/cc
@Pressure 0.276 MPa
no shim
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+15 ohm-cm
@Pressure 0.276 MPa
no shim
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.80 W/m-K
@Pressure 0.276 MPa
no shim
 
Descriptive Properties
Bond Line0.5 milno shim @ 40 psi
 no shim @ 40 psi
Thermal Impedance0.09°C cm2/Wno shim @ 40 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® Nickelvac® HC-276 Nickel Superalloy, Heat Treatment: 1121°C (2050°F) Anneal
ATI Allvac® Nickelvac® C-276 UNS N10276 Nickel Superalloy
DuPont MOLYKOTE® AS-880N GREASE
Cotronics Duralco™ 4540 Machinable Epoxy
Cotronics Duralco™ 133 500°F (260°C) Aluminum Filled Epoxy

PHONWL126 / 179671

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.