MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Filtek™ Z250 Universal Restorative Dental Composite
Categories: Polymer; Thermoset; Methacrylate

Material Notes: 3M™ Filtek™ Z250 universal restorative is an esthetic, light cured, radiopaque composite specifically designed for use in anterior or posterior direct or indirect restorations. Bonding to tooth structure is accomplished by using a dental adhesive system, such as 3M™ Single Bond or 3M™ Scotchbond Multi-Purpose Adhesive Systems. The restorative is available in a variety of shades and is packaged in traditional syringes and single dose capsules.

The matrix of this composite is a resin consisting of BIS-GMA (Bisphenol A diglycidyl ether dimethacrylate), UDMA (urethane dimethacrylate), and Bis-EMA (Bisphenol A polyethylene glycol diether dimethacrylate). This light-cured resin is filled with 60% (volume) silica/zirconia. The filler particle size distribution is 0.01 µm to 3.5 µm with an average particle size of 0.6 µm.

Filtek™ Z250 exhibits about 18% less volumetric shrinkage upon curing than 3M™ Z100™. An example from the manufacturer shows shrinkage of 2.0% after 5 minutes and 2.2% after 30 minutes; sample geometry will effect actual values. Wet fracture toughness is 1.5 MN/m. The wear rate in an in-vitro 3-body wear test gives 3.6 µLoss/39,000 cycles.

Information provided by 3M. Contact 3M for further information before specifying or using this product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 3.50e+7 cPtarget viscosity before cure
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 85.0 MPaDiametral tensile strength
Flexural Yield Strength 155 MPa
Flexural Modulus 11.0 GPa
Compressive Yield Strength 405 MPa
Adhesive Bond Strength 24.0 MPafor 2.5 mm increment. Bond strength to dentin using 3M Single Bond adhesive; C2 color
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 °CLight cured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AgPd-4 Precious dental alloy
HGC-1 Precious dental alloy
Kennametal Stellite Denertia™ C13 Cobalt Chromium Dental Alloy
Kennametal Stellite Denertia™ C14 Cobalt Chromium Dental Alloy
Kennametal Stellite Denertia™ C4 Cobalt Chromium Dental Alloy

PMMM01 / 53486

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.