MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MAR-M509 Cast Cobalt Alloy
Categories: Metal; Superalloy; Cobalt Base

Material Notes: Typical applications: jet engine blades, vanes

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.86 g/cc0.320 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  37.9 MPa
@Temperature 1090 °C,
Time 3.60e+6 sec
5500 psi
@Temperature 2000 °F,
Time 1000 hour
 55.2 MPa
@Temperature 1090 °C,
Time 360000 sec
8000 psi
@Temperature 2000 °F,
Time 100 hour
 89.6 MPa
@Temperature 982 °C,
Time 3.60e+6 sec
13000 psi
@Temperature 1800 °F,
Time 1000 hour
 117 MPa
@Temperature 982 °C,
Time 360000 sec
17000 psi
@Temperature 1800 °F,
Time 100 hour
 228 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
33000 psi
@Temperature 1500 °F,
Time 1000 hour
 269 MPa
@Temperature 816 °C,
Time 360000 sec
39000 psi
@Temperature 1500 °F,
Time 100 hour
 
Component Elements PropertiesMetricEnglishComments
Boron, B <= 0.10 %<= 0.10 %
Carbon, C 0.60 %0.60 %
Chromium, Cr 21.5 %21.5 %
Cobalt, Co <= 55.4 %<= 55.4 %Balance
Iron, Fe 1.0 %1.0 %
Manganese, Mn <= 0.10 %<= 0.10 %
Nickel, Ni 10 %10 %
Silicon, Si <= 0.10 %<= 0.10 %
Tantalum, Ta 3.5 %3.5 %
Titanium, Ti 0.20 %0.20 %
Tungsten, W 7.0 %7.0 %
Zirconium, Zr 0.50 %0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek MAR-M-509® Centri-Vac Nickel Cobalt Based Alloy
FSX-414 Cast Cobalt Alloy
Imerys NYGLOS® M15 Wollastonite
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
CMSX-2 Nickel Alloy Composition Spec

NZ97080 / 191473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.