MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® K307 MDPE Hexene Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Extruded

Material Notes: Extrusion grade hexene copolymer

Characteristics: good processability, excellent melt strength, broad fusion range, outstanding stress crack resistance, meets the requirements of GRI-GM13. Meets ASTM D4976-89 - PE 235. ASTM D1248 - Type II, Class A, Category 5.

Applications: pond liners, gas and chemical tank containment liners, landfill liners

Data provided by Chevron Phillips Chemical Company, LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.937 g/ccASTM D1505
ESCR 100% Igepal® >= 1500 hourCond. C; 100% Igepal®; F50; ASTM D1693
ESCR 10% Igepal® >= 1500 hourCond. B; F50; ASTM D1693
High Load Melt Index 21 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2900 psiType IV; 50 mm per min crosshead speed; ASTM D638
Elongation at Break >= 700 %Type IV; 50 mm per min crosshead speed; ASTM D638
Flexural Modulus 121000 psiASTM D790
 
Processing PropertiesOriginal ValueComments
Processing Temperature 193 - 232 °CExtrusion Stock

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer
Ensinger TECAPRO™ MT Medical Grade Polypropylene (PP)
Formosa Plastics Formolene® LH5204 Injection Molding HDPE
Formosa Plastics Formolene® LH5206 Injection Molding HDPE
Formosa Plastics Formolene® LH5212 Injection Molding HDPE

PCHEVM42 / 20332

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.