MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Teknor Apex Laripur® LPR 7560EG Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Features:

- Excellent performance under extreme and aggressive environments - Superior abrasion and cut resistance - Resistance to chemical, microbial attack and hydrolysis - Excellent flexibility at low temperatures - Good weathering properties - Non-halogen flame retardant

- Glossy/Transparent

- EEC Food Contact Approved

- FDA Food Contact Approved

- NSF 61 Portable Water Approved

- USP Medical Class VI

Applications:

- Energy & Power Cables: coiled or spiral: Construction / Mining - Automotive Cables: Anti-lock Braking Systems – ABS - Industrial Cables: Traffic / Signal / Trains / Boats / Buildings - Geophysical Cables: Land & Off-shore; Marine, Sub-sea & Umbilical - Telecommunications Cables: Telephone & Data Transmission; Military and Fiber Optics - Audio and Medical Cables

Information Provided by Teknor Apex

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 77ASTM D2240
Tensile Strength 6000 psiASTM D412
Tensile Stress at Strain 440 psi
@Strain 50 %
ASTM D412
 630 psi
@Strain 100 %
ASTM D412
 1200 psi
@Strain 300 %
ASTM D412
Elongation at Break 690 %ASTM D412
Tear Strength 314 kN/mASTM D624
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 158 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
Abrasion Loss (mm3)35DIN 53516

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Laripur® LPR 9060EG Thermoplastic Polyurethane
Teknor Apex Laripur® LPR 5260EG Thermoplastic Polyurethane
Hannam Chemical Hanalac 750 ABS, General Purpose
INEOS Styrolution Terlux® 2802 Transparent MABS
LG Chemical TR551 MABS, High Transparency, High Rigidity, High Hardness

PTEKNO863 / 129044

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.