MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Washington Penn PPH2TF-2B Polypropylene, 20% Talc Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Injection Molding Grade. Heat Stabilized. Meets Ford ESH-M4D293-B Spec.

Applications: AC Blower wheels, parts and appliances.

Data provided by Washington Penn Plastic Co., Inc.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Linear Mold Shrinkage 0.014 - 0.016 cm/cmASTM D955
Melt Flow 3.0 - 7.0 g/10 minCond L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 31.0 MPa50 cm/min; ASTM D638
Flexural Modulus 2.20 GPaTangent; ASTM D790
Izod Impact, Notched 0.300 J/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 115 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Washington Penn Homopolymer Polypropylene 20% Talc Filled
Washington Penn Medium Impact Copolymer 20% Talc Filled
A. Schulman TPP20AF01HB 20% Talc-Filled Homopolymer Polypropylene
Overview of materials for Polypropylene with 20% Talc Filler
LyondellBasell Hostacom™ BJ23A Polypropylene Copolymer

PWPP01 / 72784

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.