MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plaskolite Optix® CA - 51 HF UVT General Purpose Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded; Acrylic, Optical Grade, Molded

Material Notes: OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.

Information provided by Plaskolite, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cmASTM D-955
Melt Flow 23 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 8100 psiASTM D-638
Elongation at Break 2.6 %ASTM D-638
Modulus of Elasticity 419 ksiASTM D-638
Flexural Strength 14.8 ksiASTM D-790
Izod Impact, Notched 0.300 ft-lb/in
@Thickness 6.35 mm
ASTM D-256
Gardner Impact 2.00 in-lb
@Thickness 3.17 mm
Falling Weight; ASTM D-3029 GB
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°CASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 165 °FASTM D-648
Vicat Softening Point 196 °FASTM D-1525
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D-1003
Transmission, Visible 92 %ASTM D-1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Spartech Polycast UVT (Ultra-Violet Transmitting) Cell Cast Acrylic
Plaskolite Optix® CA - 75 UVT General Purpose Acrylic Resin
Plaskolite West Optix® CA - 41 UVT General Purpose Acrylic Resin
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release
Covestro Makrolon® OD2015 Polycarbonate

PPLAS960 / 150517

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.