MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Advanced Elastomer Systems VistaFlex® 641N Thermoplastic Rubber  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.

Key Features: Flex modulus (1% Secant) 7.2 MPa (1050 psi); Vicat softening point, 48°C (118°F); Melt flow rate (230°C [446°F], 2160 g [76 oz], 3.5 g [0.1 oz]/10min); Excellent PE and PP modifier for improved impact and flexibility; Smooth part appearance; Snappy 'rubber band' performance; Approved for food contact; Low rubber gel contact for film applications

Additional processing comments: Cycle times: initial inject 0.5 to 5 sec; secondary inject 1.5 to 10 sec. Initial inject pressure: high; just short of flash. Inject speed: just short of flash.

Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.

Advanced Elastomer Systems is now a part of ExxonMobil. This grade was removed from the Advanced Elastomers Systems standard product line before the ExxonMobil acquisiton.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccTPE-0105 (ASTM D792)
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 605 Second; TPE-0169 (ASTM D 2240)
Tensile Strength, Ultimate 13.5 MPaTPE-0153 (ASTM D 412)
Elongation at Break 788 %TPE-0153 (ASTM D 412)
100% Modulus 0.00160 GPa
@Strain 100 %
TPE-0153 (ASTM D 412)
Flexural Modulus, 1% Secant 0.00720 GPa
Graves Tear Strength 33.0 kN/mTPE-0056 (ASTM D 624)
Compression Set 70 %
@Temperature 23.0 °C,
Time 605000 sec
TPE-0016 (ASTM D 412)
Tensile Set 17 %23°C, 168 hrs.; TPE-0053 (ASTM D 412)
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 48.0 °C
Brittleness Temperature <= -60.0 °CTPE-0089 (ASTM D 746)
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 138 °C
Front Barrel Temperature 143 °C
Nozzle Temperature 149 °C
Melt Temperature 154 °C
Mold Temperature 21.0 - 49.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Engineered Polymers Dexflex® 756-67 TPO
Advanced Elastomer Systems Trefsin® 3201-85 W305 Thermoplastic Rubber
Advanced Elastomer Systems Vistaflex® 671N Thermoplastic Rubber
Advanced Elastomer Systems VistaFlex® 714-B Thermoplastic Rubber
Advanced Elastomer Systems VistaFlex® 714-N Thermoplastic Rubber

PADW60 / 22896

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.