MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ravago Manufacturing Americas Hylac HH23 ABS, High Heat Resistance, Medium Impact, DAM
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes:

Information provided by Ravago Manufacturing Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccISO 1183
Melt Flow  2.4 g/10 min
@Load 3.80 kg,
Temperature 230 °C
2.4 g/10 min
@Load 8.38 lb,
Temperature 446 °F
Melt Volume Rate (cm3/10min); ASTM D1238
 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
Melt Volume Rate (cm3/10min); ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 43.0 MPa6240 psiISO 527-1
Elongation at Break 15 %15 %ISO 527-1
Flexural Strength 72.0 MPa10400 psiISO 178
Flexural Modulus 2.413 GPa350.0 ksiISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²5.71 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C235 °FISO 75-2B
Deflection Temperature at 1.8 MPa (264 psi) 102 °C216 °FISO 75-2A
Vicat Softening Point 124 °C255 °FISO 306
Shrinkage, MD 0.30 - 0.70 %
@Thickness 3.17 mm
0.30 - 0.70 %
@Thickness 0.125 in
ISO 294-4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylac HH157 ABS, High Heat Resistance, Medium Impact, DAM
Techmer ES HiFill® ABS GF20 IM 20% Glass Filled
Techmer ES HiFill® ABS HI 350 High Impact
Ravago Manufacturing Americas Hyrene HI82 Polystyrene, Impact Modified, DAM
Nexeo® HIVAL® HG6 Black Acrylonitrile Butadiene Styrene

PRAVAGO1063 / 221595

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.