Description: Flow media. Ideally suited to infusion applications. Features & Benefits: - Knitted infusion mesh designed for use in vacuum assisted resin infusion processes.
- Constructed from HDPE and manufactured in a 3D knitted pattern to allow controlled resin flow across the laminate.
- Ideal for use in areas of complex tooling geometry and high temperature applications
- Allowing for a continuous air evacuation route when used with appropriate bagging materials.
Information provided by Cytec, subsequently acquired by Solvay. |