MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Wacker® AKF 10000 Non-Impact Printing
Categories: Fluid; Polymer

Material Notes: Product description: WACKER® AKF 10 000 is noted for its very low volatile content, high purity and excellent release properties.

Properties: WACKER® AKF 10 000 is a linear, non-reactive polydimethylsiloxane with a viscosity of approx. 10000 mm²/s. The chemical structure of WACKER® AKF 10 000 imparts a spectrum of special properties, which distinguish it from organic materials, e.g. mineral oils.

Application: WACKER® AKF 10 000 is used as release agents in electrophotographic equipment, such as copiers, laser printers etc.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 - 0.980 g/cc
Volatiles 0.50 %
@Temperature 200 °C,
Time 86400 sec
10g / procelain dish, diameter 9.6 cm, circulating air)
Viscosity 1000 cPdynamic
 
Thermal PropertiesOriginal ValueComments
Pour Point -50.0 °CDIN ISO 3016
Flash Point >= 300 °CDIN 51376
Ignition Temperature 450 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.404DIN 51423

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9729 / 205258

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.