MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Lehvoss LUVOCOM® 1301-7449 PPS, linear with carbon fiber and PTFE
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler

Material Notes: Properties/attributes include: High-strength and stiffness parts with low creep. Improved friction and wear behavior. Emergency (dry) running property. Electrically conductive, suitable for continuous discharging of statically-generated electricity. High continuous-use and heat-distortion temperatures. Non flammable.

Automotive industry, textile-and office machinery, medical- and precision engineering. Typical uses include: Control disks, gear wheels, pump impellers, gear parts for automotive appliances, chip carrier.

Processing: The material does not necessarily have to be predried; when originally sealed containers are used, this process may normally be omitted. Processing temperatures above 360°C may very rapidly cause thermal damage and should therefore be avoided. Post-crystallization may lead to warpage at elevated operating temperatures. This can be counteracted by suitable heat treatment. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application. High-temperature polymers place increased demands on the tool steels employed.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.54 g/ccISO 1183
Moisture Absorption <= 0.100 %
@Temperature 23.0 °C,
Time 86400 sec
Linear Mold Shrinkage 0.00050 - 0.0020 cm/cmDIN 16901
Melt Flow 10 g/10 min
@Load 10.0 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 180 MPaISO 527-2
Elongation at Break 1.0 %ISO 527-2
Modulus of Elasticity 25.0 GPaISO 527-2
Flexural Strength 270 MPaISO 178
Flexural Modulus 22.0 GPaISO 178
Flexural Strain at Break 1.3 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 25.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eU
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 1000 ohm-cmIEC 60167
Surface Resistance <= 100 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µm/m-°CDIN 53752
Thermal Conductivity 0.750 W/m-KDIN 52612
Maximum Service Temperature, Air 220 °CContinuous; UL 746B
 240 °CShort Term
Vicat Softening Point 240 °CVST A; DIN ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 320 - 340 °C
Zone 1 300 - 320 °C
Zone 2 310 - 330 °C
Zone 3 320 - 340 °C
Melt Temperature 330 °C
Mold Temperature 150 - 180 °C
Drying Temperature 50.0 - 90.0 °C
@Time >=14400 sec
 100 - 140 °C
@Time 7200 - 14400 sec
Dehumidifying dryer
 
Descriptive Properties
Colornatural color (black)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 2139 Composition Spec
7449 Aluminum Composition Spec
RTP Company RTP 1385 D TFE 10 Polyphenylene Sulfide (PPS), Carbon Fiber - PTFE Lubricated
2519 Aluminum Composition Spec
Carlisle 201LD Carbon-Carbon Composite

PLUU8874 / 193833

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.