MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Danquinsa DANADD® E-LF-01 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANADD® E-LF-01 is a concentrated additive Masterbatch which is added to thermoplastic polyurethanes and also to other plastics in order to obtain a good electrical conductivity. DANADD® E-LF-01 contains thermoplastic polyurethane as a binder. DANADD® E-LF-01 is added into the TPU-pellets by a metering equipment and by mixing it with the TPU-pellets. In the production of lightweight-TPU, it is also possible to mix DANADD® E-LF-01 with colour- and additive masterbatches ( Expander additives ).

Application: DANADD® E-LF-01 can be added to TPU-pellets if they are processed by extrusion, blow-moulding and injection-moulding. By adding DANADD® E-LF-01, the TPU’s obtain a good electrical conductivity. This product is applied in the production of rollers, shoe soles or speciality profiles based on TPU, if these products need to have a good electrical conductivity. For application in TPU’ s, the inherent colour of DANADD® E-LF- 01 enables another colouring by addition of masterbatches. Depending on its application and the electrical conductivity required, 1 – 25 % of DANADD® E-LF-01 are added to the granules.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 15.0 - 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Softening Point 135 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 135 - 230 °C
Moisture Content <= 0.050 %Residual
Shelf Life 6.00 Month
 
Descriptive Properties
Active content0.5
AspectGrey to black, irregular (inhomogeneous) cylindrical granules

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ003 / 294423

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.