MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil HPA 020 Wire & Cable High Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HPA 020 is a HDPE grade for Medium/High Voltage power cable jacketing. The grade should be used in blends with LLDPE to improve ESCR. Sufficient Carbon Black or UV stabilizer should be added to meet cable jacketing specifications.

Availability: Africa & Middle East, Asia Pacific and Europe

Applications:

  • Automotive wiring compounds
  • MV/HV thermoplastic jacketing
  • Telecom/Data/ LAN cable insulation

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³ASTM D4883
Melt Flow 9.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
9.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 62
@Time 15.0 sec
62
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 33.1 MPa4800 psiASTM D638
Tensile Strength, Yield 26.9 MPa3900 psiASTM D638
Elongation at Break 840 %840 %ASTM D638
Elongation at Yield 9.0 %9.0 %ASTM D638
Flexural Modulus, 1% Secant 896 MPa130000 psiASTM D790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.20e+15 ohm-cm6.20e+15 ohm-cmASTM D257
Dielectric Constant 2.2
@Frequency 60 Hz
2.2
@Frequency 60 Hz
ASTM D150
Dielectric Strength 55.1 kV/mm1400 kV/in500 V/sec; ASTM D149
Dissipation Factor 0.00050
@Frequency 60 Hz
0.00050
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 129 °C264 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SCG Chemicals EL-Lene™ H2001WC High Density Polyethylene Wire & Cable Grade
Global BM-3245-PC High Density Polyethylene, Pipe Extrusion Grade
Dow HDPE 30460M High Density Polyethylene
Eastman M3006-P Polyethylene
Eastman M30036-P Polyethylene

PEX99321 / 175557

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.