MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex APEX® 1003 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Wire and Cable Grade

Material Notes: Notes: 60°C General Purpose; RoHS Compliant

Uses: Connectors; Grommets; Plugs; Strain Reliefs

Forms: Pellets

Processing Method: Injection Molding

Agency Ratings: UL QMFZ2 .E54709

Wire Types: Molded Components

Additional Information:

Temperature Rating: 60°C

Recognized Component, CSA C22.2 No. 0.6, CSA Flammability Classification: 0.6HB at 0.88mm

Information Provided by Teknor Apex

Key Words: PVC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
Linear Mold Shrinkage 0.010 - 0.012 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 7915 seconds; ASTM D2240
Tensile Strength at Break 1530 psiASTM D638
Elongation at Break 260 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index >= 600 V
@Thickness 3.00 mm
UL 746
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness 3.00 mm
UL 746
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness 3.00 mm
UL 746
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 140 °FContinuous Use; ASTM D794
Brittleness Temperature -31.0 °FASTM D746
UL RTI, Electrical 194 °F
@Thickness 0.889 mm
UL 746
 194 °F
@Thickness 1.40 mm
UL 746
 194 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 176 °F
@Thickness 0.889 mm
UL 746
 194 °F
@Thickness 1.40 mm
UL 746
 194 °F
@Thickness 3.00 mm
UL 746
Flammability, UL94 HB
@Thickness 0.889 mm
 HB
@Thickness 1.40 mm
 HB
@Thickness 3.00 mm
Oxygen Index 24 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 355 °FProcessing Temperature
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex APEX® 01-A0087A-91 Polyvinyl Chloride, Flexible
Teknor Apex APEX® 02-A0033A-65 NT1 Polyvinyl Chloride, Flexible
Teknor Apex APEX® 1002 Polyvinyl Chloride, Flexible
Teknor Apex APEX® 94-A0098C-90 Polyvinyl Chloride, Flexible
Teknor Apex APEX® 04-A0386B-88 Polyvinyl Chloride, Flexible

PTEKNO547 / 128725

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.