MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum 7075-O
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: General 7075 characteristics and uses (from Alcoa): Very high strength material used for highly stressed structural parts. The T7351 temper offers improved stress-corrosion cracking resistance.

Uses: Aircraft fittings, gears and shafts, fuse parts, meter shafts and gears, missile parts, regulating valve parts, worm gears, keys, aircraft, aerospace and defense applications.

Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
A Zr + Ti limit of 0.25 percent maximum may be used with this alloy designation for extruded and forged products only, but only when the supplier and the purchaser have mutually agreed.
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A97075; ISO AlZn5.5MgCu(A); Aluminium 7075-O; AA7075-O; Al7075-O
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.81 g/cc0.102 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 6060AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 8080Converted from Brinell Hardness Value
Hardness, Vickers 6868Converted from Brinell Hardness Value
Tensile Strength, Ultimate 228 MPa33000 psiAA; Typical
 <= 276 MPa<= 40000 psiSheet and plate
Tensile Strength, Yield 103 MPa15000 psiAA; Typical
 <= 145 MPa<= 21000 psiSheet and plate
Elongation at Break >= 10 %>= 10 %Sheet and plate
 17 %
@Thickness 1.59 mm
17 %
@Thickness 0.0625 in
AA; Typical
 16 %
@Diameter 12.7 mm
16 %
@Diameter 0.500 in
AA; Typical
Modulus of Elasticity 71.7 GPa10400 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Poissons Ratio 0.330.33
Shear Modulus 26.9 GPa3900 ksi
Shear Strength 152 MPa22000 psiAA; Typical
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000380 ohm-cm0.00000380 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.6 µm/m-°C
@Temperature -50.0 - 20.0 °C
12.0 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.4 µm/m-°C
@Temperature 20.0 - 100 °C
13.0 µin/in-°F
@Temperature 68.0 - 212 °F
 23.6 µm/m-°C
@Temperature 20.0 - 100 °C
13.1 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 24.3 µm/m-°C
@Temperature 20.0 - 200 °C
13.5 µin/in-°F
@Temperature 68.0 - 392 °F
 25.2 µm/m-°C
@Temperature 20.0 - 300 °C
14.0 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.960 J/g-°C0.229 BTU/lb-°F
Thermal Conductivity 173 W/m-K1200 BTU-in/hr-ft²-°F
Melting Point 477 - 635.0 °C890 - 1175 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness. Homogenization may raise eutectic melting temperature 20-40°F but usually does not eliminate it.
Solidus 477 °C890 °FAA; Typical
Liquidus 635.0 °C1175 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 413 °C775 °F
Solution Temperature 466 - 482 °C870 - 900 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 87.1 - 91.4 %87.1 - 91.4 %As remainder
Chromium, Cr 0.18 - 0.28 %0.18 - 0.28 %
Copper, Cu 1.2 - 2.0 %1.2 - 2.0 %
Iron, Fe <= 0.50 %<= 0.50 %
Magnesium, Mg 2.1 - 2.9 %2.1 - 2.9 %
Manganese, Mn <= 0.30 %<= 0.30 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.40 %<= 0.40 %
Titanium, Ti <= 0.20 %<= 0.20 %
Zinc, Zn 5.1 - 6.1 %5.1 - 6.1 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 7075-T6; 7075-T651
Aluminum 6061-O
Aluminum 7075-T73; 7075-T735x
Alclad Aluminum 7075-T6, T651
Alclad Aluminum 7075-O

MA7075O / 9594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.