MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestodur® GF50 nf PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled

Material Notes: For the injection molding of very rigid and heat resistant parts.

ISO data as provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.71 g/cc
Water Absorption 0.00 %
Moisture Absorption at Equilibrium <= 0.50 %Humidity Absorption
Melt Flow 8.0 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 160 MPa
Elongation at Break 1.0 %
Modulus of Elasticity 15.0 GPa
Charpy Impact Unnotched 6.00 J/cm²
 6.50 J/cm²
@Temperature -30.0 °C
Charpy Impact, Notched 1.30 J/cm²
 1.20 J/cm²
@Temperature -30.0 °C
Tensile Impact Strength 80.0 kJ/m²
Tensile Creep Modulus, 1 hour 15000 MPa
Tensile Creep Modulus, 1000 hours 10000 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
Dielectric Constant 4.0
@Frequency 100 Hz
 4.0
@Frequency 1e+6 Hz
Dielectric Strength 27.0 kV/mm
Dissipation Factor 0.0040
@Frequency 100 Hz
 0.015
@Frequency 1e+6 Hz
Comparative Tracking Index 500 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow <= 50.0 µm/m-°C
@Temperature 20.0 °C
CTE, linear, Transverse to Flow <= 50.0 µm/m-°C
@Temperature 20.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
Vicat Softening Point 215 °C50°C/hr/50 N
UL RTI, Electrical 130 °C
UL RTI, Mechanical with Impact 130 °C
UL RTI, Mechanical without Impact 140 °C
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical Lupox® SG5500 PBT+PET+GF50%
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT
Celanese Crastin® SK609 NC010 PBT-GF50
Envalior Arnite® TV4 290 PBT-GF50
Celanese Celstran® PBT-GF50-08 PBT, 50% Glass Reinforced

PHUM20 / 47453

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.