MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Multibase Multi-Pro® 1010 T Black 10% Talc Content Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Talc Filler

Material Notes: PPH talc filled compound suitable for containers and wash-tubs requiring elevated stiffness and improved cycle times.

Data provided by Multibase.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.974 g/ccASTM D792-91
Melt Flow 11 g/10 min(Condition L) ASTM D-1238-94a
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 33.8 MPaASTM D638-95
Elongation at Break 60 %ASTM D638-95
Flexural Strength 46.9 MPaASTM D790-92
Flexural Modulus 2.00 GPaMethod 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.480 J/cmASTM D256-93a
Gardner Impact 0.700 JASTM D5420-93

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Multibase Multibatch® ME 50024 Sheet Extrusion
Multibase Multibatch® ME 50003 Anti-blocking Masterbatch
Multibase Multi-Pro® 4006 T H BLK 40% Talc Content Polypropylene
Multibase Multibatch® MP 52577 Sheet Extrusion
Multibase Multibatch® MP 52206 Sheet Extrusion

PLA249 / 49646

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.