MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CeramTec 614/698 Alumina, 96%
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: 614/698 (96%) is a high-strength alumina with good mechanical properties, as well as good wear and chemical resistance. It also features excellent electrical properties. 614 is white; 698 is pink.

Key Words: Al2O3, aluminum oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.70 g/ccDIN EN 623-2 / ASTM-C373 / ASTM-C20
Water Absorption 0.00 %DIN EN 623-2 / ASTM-C373
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 1200HV 0.5; DINV ENV 843-4
Tensile Strength at Break 172 MPaACMA Test #4 / DIN EN 843-1
Tensile Modulus 276 GPaYoung's; DINV ENV 843-2 / ASTM-F417
Flexural Strength 276 MPa20 x 40 mm
Compressive Strength 2414 MPaASTM C-773-88 / DIN 51067T1
Poissons Ratio 0.24DINV ENV 843-2
Fracture Toughness 2.70 MPa-m½DIN 51109
Shear Modulus 128 GPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 680000 ohm-cm
@Temperature 900 °C
 7.30e+7 ohm-cm
@Temperature 500 °C
 2.00e+13 ohm-cm
@Temperature 100 °C
IEC 672-1
 >= 1.00e+14 ohm-cm
@Temperature 25.0 °C
ASTM-D257
Dielectric Constant 9.3
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-C150
Dielectric Strength 8.268 kV/mm6.35 mm (1/4") IEC 672-1
Dissipation Factor 0.00030
@Frequency 1e+6 Hz
 0.00090
@Frequency 1e+10 Hz
 0.00090
@Frequency 2.50e+10 Hz
Dielectric Loss Index 0.0028
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-D149,150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.90 µm/m-°CDIN EN 821-1
 6.40 µm/m-°C
@Temperature 20.0 - 200 °C
 7.50 µm/m-°C
@Temperature 20.0 - 600 °C
ASTM-C373
 8.00 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.900 J/g-°C
@Temperature 100 - 200 °C
DINV ENV 821-3
Thermal Conductivity 35.2 W/m-KDIN EN 821-2 / ASTM-C408
Maximum Service Temperature, Air 1500 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 96 %
 
Descriptive Properties
ColorWhite/Pink
Te Value (°C)840
Thermal Shock Resistance R1 (K)200Hasselman (Experimental)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec Rubalit® 708S Alumina, 96%
CeramTec V 679 Alumina, 99.7%
Overview - Alumina, 96%, Al2O3
CeramTec 975 Alumina, 99.5%
CeramTec B 40 Alumina, 99.1%

CCERA930 / 107530

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.