MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical SEETEC PH150 HDPE Blown Film Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Features: Characteristics : Excellent weather resistance & Environmental stress cracking resistance
Additives : Anti-Oxidants, Lubricants
Processing recommendations : Maintain the stock temperature 200-230°C (392-446°C) for optimum part quality

Application: Pressure pipes for water and drainage (Base resin)

Specification Data
1) Cell Class (ASTM D 1248) : Type ?, Class A, Category 5, Grade P34
2) Cell Class (ASTM D 3350) : 34544(ESCR:>600hr)4 A or 34546(PENT:>100hr)4 A
3) PPI Recommended Designation : PE3408
4) ISO Classification : Grade PE80

CAS No. 25213-02-9

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.942 - 0.945 g/ccASTM D1505
Environmental Stress Crack Resistance >= 1500 hourF50; ASTM D1693
Melt Flow 0.10 - 0.15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 54ASTM D785
Tensile Strength at Break 35.0 MPa50mm/min; ASTM D638
Tensile Strength, Yield 220 kg(f)/cm²50 mm/min; ASTM D638
Elongation at Break >= 800 %
@Thickness 50.0 mm
ASTM D638
Flexural Modulus 9000 kg(f)/cm²ASTM D790
Izod Impact, Unnotched >= 20.0 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 128 °C10°C/min; ASTM D3418
Vicat Softening Point 123 °CASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Heraeus Clevios™ P VP CH 8000 Conductive Sulfonate Polymer for Antistatic Coatings
Borealis HE1878 High Density Polyethylene Powder for Crosslinked Pipes
LG Chemical LUTENE-H XL1800 HDPE
Baystar™ 2287 HDPE Bimodal Film Resin
Kraton® D1102 + HDPE blend (10/90)

PLAY208 / 148218

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.