System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
3M Dyneon™ CC605 PTFE 25% Fiberglass Filled
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Fluoropolymer
;
Polytetrafluoroethylene (PTFE)
;
Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Material Notes:
Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.
Data provided by Dyneon.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Bulk Density
0.730
g/cc
ASTM D4894
Density
2.22
g/cc
ASTM D4894
Particle Size
750
µm
ASTM D4894
Deformation
3.0 %
@Pressure 15.00 MPa
ASTM D621
7.0 %
@Time 86400 sec,
Pressure 15.00 MPa
ASTM D621
Mechanical Properties
Original Value
Comments
Hardness, Shore D
57
value after 15 sec; ASTM D2240
62
initial value; ASTM D2240
Tensile Strength at Break
17.2
MPa
ASTM D4894
Elongation at Break
230 %
ASTM D4894
Tensile Modulus
23000
psi
ASTM D638
Thermal Properties
Original Value
Comments
CTE, linear
50.0
µm/m-°C
@Temperature 30.0 - 100 °C
ASTM E831
68.0
µin/in-°F
@Temperature 100 - 200 °C
ASTM E831
84.0
µin/in-°F
@Temperature 200 - 300 °C
ASTM E831
Thermal Conductivity
0.290
W/m-K
@Temperature 100 °C
ASTM E1530
0.300
W/m-K
@Temperature 250 °C
ASTM E1530
Shrinkage
1.6 %
ASTM D4894
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
AGC Fluon® FC 405 PTFE, 25% Glass Fiber Filled
AGC Fluon® FP-EF-105 PTFE, 25% Glass Filled
AGC FC 405 PTFE, 25% Glass Fiber
AGC Fluon® RB1025S 25% Glass Fiber, PTFE Filled Compound
AGC FC 403 PTFE, 15% Glass Fiber
PDYM67 / 34679
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.