MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Armacell Monarch® F-05055 (Black) Neoprene, EPDM, SBR Blend Foam
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • UL94 HF-1 and HBF listed for flame
  • ASTM D 1056-07 2A5 grade material
  • Fine cell – manufactured in blocks (buns)
  • Widely used general purpose EPDM/CR/SBR blend, an industry standard
  • UL50E (periodic and continuous compression), UL508 and UL48 listed for gaskets and seals (recent upgrade)

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 10.0 - 14.0 lb/ft³ASTM D1056
Water Absorption <= 5.0 %ASTM D1056
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 65 - 75ASTM D2240
Tensile Strength 150 psiASTM D412, Die A
Elongation at Break 125 %ASTM D412, Die A
Compressive Strength 17.0 - 25.0 psi
@Strain 25 %
ASTM D1056
Resilience 15[%]; ASTM D2632
Tear Strength >= 35.0 pliDie C; ASTM D624
Compression Set <= 25 %ASTM D1056
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °FContinuous; ASTM D746
 250 °FIntermittent; ASTM D746
Minimum Service Temperature, Air -40.0 °FASTM D746
Flammability, UL94 HB
@Thickness 45.7 mm
 
Descriptive Properties
Accelerated Aging±30%Change in Compression Deflection, 7 days at 70°C, ASTM D1056
ColorBlack
FlammabilityFMVSS302Pass at >1.75 mm
 HF-11.5-1.8 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow SE BR-1220L Stereospecific high cis-1,4 Polybutadiene (BR)
Nitriflex SB-1011 Styrene Butadiene Copolymer
Nitriflex SB-1011G Styrene Butadiene Copolymer
Armacell Monarch® F-05091 (Black) Neoprene, EPDM, SBR Blend Foam
Armacell Monarch® F-05031 (Black) Neoprene, EPDM, SBR Blend Foam

PARMD102 / 186713

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.