MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Fiberloc™ 82510 PVC, Rigid with 10% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, 10% Glass Fiber Reinforced; PVC, Rigid Grade

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccASTM D792
Filler Content 10 %Glass Fiber
Linear Mold Shrinkage, Flow 0.00050 - 0.0015 cm/cmASTM D955
Spiral Flow 53.3 cmRelative Spiral Flow; 23
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83ASTM D2240
Tensile Strength, Yield 62.1 MPaType I, 51 mm/min; ASTM D638
Elongation at Break 3.0 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 4830 MPaType I, 51 mm/min; ASTM D638
Flexural Strength 103 MPaASTM D790
Flexural Modulus 4480 MPaASTM D790
Poissons Ratio 0.42ASTM E132
Shear Modulus 1.70 GPaCalculated
Izod Impact, Notched 53.4 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.18 mm
Injection Molded; ASTM D4812
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 41.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C
@Thickness 6.35 mm
Annealed; ASTM D648
UL RTI, Electrical 50.0 °CUL 746
UL RTI, Mechanical with Impact 50.0 °CUL 746
UL RTI, Mechanical without Impact 50.0 °CUL 746
Flammability, UL94 V-0
@Thickness 1.47 mm
All colors; UL 94
 5VA
@Thickness 1.47 mm
All colors; UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 210 °C
 
Descriptive Properties
Agency RatingsNSF 61
FeaturesGeneral Purpose
 Medium Flow
FormsPellets
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesFluid Handling
 General Purpose

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions 83530 Fiberloc PVC; 30% Glass Fiber Reinforced
Geon® Performance Solutions 83520 Fiberloc PVC; 20% Glass Fiber Reinforced
Geon® Performance Solutions 82530 Fiberloc PVC; 30% Glass Fiber Reinforced
Geon® Performance Solutions 82520 Fiberloc PVC; 20% Glass Fiber Reinforced

PH1PN8181 / 102017

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.