MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NYCOA 2047 Copolymer Nylon 6/69
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/69

Material Notes: extrusion, high melt viscosity. & strength., low crystallinity

Information provided by NYCOA, Inc.

Key Words: PA 6/69, Polyamide 6/69, Nylon 6/69
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccASTM D792
Water Absorption 1.7 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 62.0 MPaASTM D638
Elongation at Break >= 300 %ASTM D638
Flexural Yield Strength 71.0 MPaISO METHOD 176
Flexural Modulus 1.903 GPaASTM D790
Izod Impact, Notched 0.700 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 199 °CASTM D789
 
Processing PropertiesOriginal ValueComments
Processing Temperature 250 °C
Rear Barrel Temperature 200 °C
Middle Barrel Temperature 230 °C
Front Barrel Temperature 250 °C
Drying Temperature 76.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NYCOA 2046 Copolymer Nylon 6/69
NYCOA 400 PA 6
Overview of materials for Nylon 11, Unreinforced
AdvanSix Aegis® H8202NLB Extrusion Grade Nylon 6
BASF Ultramid® C33 PA6/66

PNYCOA18 / 55564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.