MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hostacom™ BC142/1AC Polypropylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Description: Hostacom™ BC142/1AC conventional melt flow, 3,600 MPa flexural modulus, precolored, mineral-filled polypropylene copolymer has a good balance of stiffness and impact resistance. It was designed primarily for structural automotive interior components that require high rigidity and low odor. Uses: Automotive interior parts

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccISO 1183
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 96ISO 2039-2
Tensile Strength, Yield 4790 psiISO 527-1, -2
Elongation at Break 70 %ISO 527-1, -2
Elongation at Yield 6.0 %ISO 527-1, -2
Flexural Modulus 522000 psiISO 178
Izod Impact, Notched (ISO) 1.70 kJ/m²
@Temperature -40.0 °C
ISO 180
 2.70 kJ/m²
@Temperature 10.0 °C
ISO 180
 3.70 kJ/m²
@Temperature 23.0 °C
ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 259 °FUnannealed; ISO 75B-1, -2
Shrinkage 0.80 %Tool, 100x150x3.2 mm; Basell Test Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostacom™ 62F4-2C Polypropylene Homopolymer
LyondellBasell Hostacom™ 63A6-4 Polypropylene Homopolymer
LyondellBasell Hostacom™ AE716BC Polypropylene Homopolymer
LyondellBasell Hostacom™ 6551 Polypropylene Homopolymer
LyondellBasell Hostacom™ BG722AC Polypropylene Copolymer

PMO809 / 53798

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.