MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TEGO® Antifoam AS 10 Emulsion
Categories: Other Engineering Material

Material Notes: Product description: TEGO® Antifoam AS 10 is an antifoam emulsion, based on organo-modified siloxanes.

Application: Due to the special combination of modified siloxanes, TEGO® Antifoam AS 10 can be used for foam control in a variety of aqueous applications.

Properties / Benefits: The special combination of active ingredients provides TEGO® Antifoam AS 10 with excellent stability in alkaline or electrolyte media, even at elevated temperatures. With regard to compatibility, dispersability and handling TEGO® Antifoam AS 10 performs much better than conventional silicone antifoams. Due to its excellent dispersability TEGO® Anti-foam AS 10 must be used as delivered.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/cc
Viscosity 130 - 520 cP
 
Descriptive Properties
Appearancewhite
Content10%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik BREAK-THRU® AF 9908 Surfactants
Evonik SIPERNAT® 383 DS Silica Powder
Evonik SIPERNAT® D 10 Ceramic Powder
Evonik SIPERNAT® 50 Silica Powder
Evonik SIPERNAT® 35 Silica Powder

PEVONIL552 / 196756

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.