MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPR 8473 Polypropylene, Film Extrusion Grade
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Random copolymer heat sealable film grade

Color/Clarity/Impact - FINA 8473 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.

Heat Sealable - The very low melting point of FINA 8473 makes it an excellent heat seal layer for oriented films.

Slip/Antiblock - FINA 8473 is available with custom slip and antiblock packages.

FDA - FINA 8473 complies with all applicable FDA regulations Title 21 CFR Section 177.1520(c) 3.1 and may be used under these provisions for food contact and packaging.

Recommended Applications - FINA 8473 is recommended for use in non- oriented film processes for manufacture of packaging films that require improved optical and impact properties and as a heat seal layer for oriented films

Processing - FINA 8473 resin processes on film extrusion equipment with typical melt temperatures of 390- 450°F (199-232°C).

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Permeability 14.0 g mil/ (m2 day)
@Temperature 37.8 °C
90% RH; ASTM E96
Density 0.895 g/ccASTM D1505
Melt Flow 4.6 g/10 minConditions not specified; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 500 %Non-oriented film; ASTM D882
Secant Modulus 0.480 GPa1% Secant Modulus; Non-oriented Film; ASTM D882
Dart Drop 9.40 g/micronF50; ASTM D 1709
Seal Strength >= 200 g/25 mmat 135°C, 15 psi pressure and 1 sec.
Film Tensile Strength at Break, MD 20.0 MPaNon-oriented film; ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 134 °CDSC
 
Optical PropertiesOriginal ValueComments
Haze 2.0 %Non-oriented film; ASTM D1003
Gloss 85 %45°; Non-oriented film; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 232 °Cfilm extrusion
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 3860X Polypropylene, Extrusion Grade
Total 3868 Polypropylene, Extrusion Grade
Total PPR 8573 Polypropylene, Film Extrusion Grade
Total PPR 7450HC Polypropylene, Film Extrusion Grade
Total PPR 7525MZ Polypropylene, Injection Molding Grade

PFIN48 / 38378

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.