MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo VYLOPET® EMC355 Injection Molding Polyester Resin, Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Applications:
  • Housings
  • Brackets
  • Gear cases
Features:
  • High Rigidity
  • Glass fiber reinforcement

Information provided by Toyobo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.81 g/cc0.0654 lb/in³ASTM D792
Water Absorption 0.050 %0.050 %ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inMD
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ASTM D785
Tensile Strength at Break 185 MPa26800 psiASTM D638
Elongation at Break 1.5 %1.5 %ASTM D638
Flexural Strength 280 MPa40600 psiASTM D790
Flexural Modulus 18.0 GPa2610 ksiASTM D790
Izod Impact, Notched 1.00 J/cm1.87 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Strength 25.0 kV/mm
@Thickness 2.00 mm
635 kV/in
@Thickness 0.0787 in
ASTM D149
Arc Resistance 130 sec130 secTungsten electrode; ASTM D495
Comparative Tracking Index 175 - 249 V175 - 249 VIEC Pub1.112, class 3; IEC Method
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C
@Temperature 20.0 °C
11.1 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Melting Point 255 °C491 °FBy DSC
Maximum Service Temperature, Air 130 °C266 °FThermal index; ASTM UL746B
 225 °C437 °FBall pressure temperature; IEC Method
Deflection Temperature at 0.46 MPa (66 psi) 245 °C473 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 235 °C455 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 255 - 270 °C491 - 518 °F
Mold Temperature 90.0 - 120 °C194 - 248 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Toyobo VYLOPET® EMC130-20 Injection Molding Polyester Resin, Flame Resistant
Toyobo VYLOPET® EMC310 Injection Molding Polyester Resin
Toyobo VYLOPET® EMC341 Injection Molding Polyester Resin, Hydrolysis Resistant
Intercontinental Polymers HoPET 720 Film Grade Resin, Clear, Polyester Pellets
Indorama AlphaPet Preformance® 1708HS(A) PET Resin

PTOY643 / 70803

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.