MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical GOYENCHEM-840 High-Effective Water & Oil Resistant / Anti-Stain Agent for Textile
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: With strong technology in fine chemicals and long-term marketing experience in industries,GO YEN CHEMICAL INDUSTRIAL CO., LTD. develops and manufactures the unique products—High Effective Nano-meter Water & Oil Resistant Agent, GOYENCHEM-840 for versatile textiles. GOYENCHEM-840 , is designed by GO YEN CHEMICAL INDUSTRIAL CO., LTD., is a kind of water based higheffective nano-meter water & oil resistant agent for different sorts of fabric finishing, including natural fabrics, synthetics fabrics and blended fabrics products, etc. GOYENCHEM-840 is able to provide perfect water & oil resistant effect and offer strong durability. However, textiles after treated with GOYENCHEM-840 will give a soft touching and feeling. Our GOYENCHEM-840 obtains a well reputation from many textile producers of Europe, Japan and U.S.A. and become an assigned brand. Most water resistant for fabrics or textiles only repel water for a limited time. Distinguished from other products, GOYENCHEM-840 is unique designed not only to provide excellent but also permanent water & oil resistant effects. Most water-resistant fabrics shed water with a short time or offer not good effect of water resistant effect because of their weave or because they treated other brand of products. However, to treat our GOYENCHEM-840 is more effective than other brand water-resistant. Fabrics coated with a finish of GOYENCHEM-840 will make the water to make beads and keep them stand-up when it hits the fabric rather than going through. The fabrics to coat our GOYENCHEM-840 will keep water resistant effect and offer durability.

Advantages:

  • Outstanding soft handling and feeling
  • Offer perfect Water & Oil Resistant properties to versatile textiles, such as natural fabrics & synthetic fabrics
  • Can better and provide excellent permeability and moistening ability to fabrics with bad moistening and high-speed processing
  • Strong adhesion to processing surface and well compatible to most of the resins, processing agents, softening agents and catalysts
  • To add dyeing additives or proceeding agents during pre-processing does not affect the properties of water & oil repellency of GOYENCHEM-840
  • Not affect original coloring, fixing, dyeing, etc.
  • Own a good stability and can be suitable to various kinds of fabrics

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
AppearanceMilk white liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN219 / 266527

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.