MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay CYCOM® E773FR Epoxy + Unidirectional Carbon Tape Prepreg
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: CYCOM® E773/E773FR resins are controlled flow epoxy systems with a large processing window. They exhibit excellent high temperature performance up to 180°F (82°C) wet service temperature. The systems have good retention of tack and drape up to 20 days at room temperature in prepreg form. A straight two hour ramp cure in either a press or an autoclave may be used. No post-cure is requirement to achieve service temperature.

Features & Benefits:

  • 250°F (121°C) cure
  • 180°F (82°C) wet service temperature
  • Low exotherm profile
  • Controlled flow
  • Large processing window
  • Available in both flame retardant (FR) and non-flame retardant grades
  • Autoclave or press mold processing
  • Available in unidirectional tape, fabric, roving, slit tape and cross-plied forms
  • History of performance on helicopter blades and other structural components
  • Shelf life of 12 months at 0°F (-18°C), 20 days at 72°F (22°C)
Applications:
  • Helicopter blades
  • Other aircraft structural components
Property data typical for laminates with cured ply thickness of 0.0056 inches for E773FR resin with AS4 12K 145 Unidirectional Tape, Standard Modulus Carbon Fiber (33 Msi/228 GPa). 'Wet' Mechanical property data are for samples conditioned 160°F (71°C) and 90% RH to 1% moisture.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 270000 - 290000 psi
@Temperature 82.0 °C
0°, wet
 285000 - 310000 psi
@Temperature 23.0 °C
0°, wet
 295000 - 310000 psi
@Temperature 23.0 °C
 290000 - 330000 psi
@Temperature -54.0 °C
Tensile Modulus 124 - 138 GPa
@Temperature 82.0 °C
0°, wet
 131 - 145 GPa
@Temperature -54.0 °C
 131 - 145 GPa
@Temperature 23.0 °C
 131 - 145 GPa
@Temperature 23.0 °C
0°, wet
Compressive Strength 862 - 1034 MPa
@Temperature 82.0 °C
0°, wet
 1172 - 1310 MPa
@Temperature 23.0 °C
0°, wet
 1206 - 1344 MPa
@Temperature 23.0 °C
 1344 - 1551 MPa
@Temperature -54.0 °C
Compressive Modulus 117000 - 131000 MPa
@Temperature 82.0 °C
0°, wet
 131000 - 145000 MPa
@Temperature -54.0 °C
 131000 - 145000 MPa
@Temperature 23.0 °C
 131000 - 145000 MPa
@Temperature 23.0 °C
0°, wet
Shear Strength 6000 - 8000 psi
@Temperature 82.0 °C
0° Interlaminar, wet
 7000 - 9000 psi
@Temperature 82.0 °C
± 45° In-plane, wet
 8000 - 10000 psi
@Temperature 23.0 °C
0° Interlaminar, wet
 9000 - 11000 psi
@Temperature 23.0 °C
± 45° In-plane, wet
 10000 - 13000 psi
@Temperature 23.0 °C
0° Interlaminar
 12000 - 14000 psi
@Temperature -54.0 °C
± 45° In-plane
 12000 - 15000 psi
@Temperature -54.0 °C
0° Interlaminar
 14000 - 16000 psi
@Temperature 23.0 °C
± 45° In-plane
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °Fwet service
Glass Transition Temp, Tg 115 °Cwet
 155 °Cdry
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 °F
@Time 5400 sec
plus ramp up and cool down
Shelf Life 0.667 Month
@Temperature 22.2 °C
 12.0 Month
@Temperature -17.8 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay CYCOM® 5320-1 Epoxy with T40/800B Unidirectional Tape Composite
Solvay CYCOM® 977-3 Epoxy - Unidirectional Carbon Fiber Tape
Solvay CYCOM® 5250-4 RTM BMI Resin, Composite with IM7-6K-4HS Fabric
Solvay CYCOM® 5250-4 RTM BMI Resin, Composite with T650-35-3K-PW Fabric
Solvay CYCOM® 890 RTM Resin - Woven Carbon Fabric Composite

PCYTED100a / 234734

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.