MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Vinnol® H 40/43 TF Vinyl Chloride Copolymer
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: CAS NO. 9003-22-9

Product description: VINNOL® H 40/43 TF is a copolymer of approx. 66 wt.% vinyl chloride (VC) and approx. 34 wt.% vinyl acetate (VAc). Its main use is as a binder for surface coating compounds and printing inks.

Properties: VINNOL® H 40/43 TF is a thermoplastic, physically drying binder that forms a film when the solvent contained in the formulation has evaporated. Like all VC copolymers, VINNOL® H 40/43 TF is extremely tough, showing permanent flexibility, abrasion resistance, little tendency to swell in the presence of water and low gas permeability. It is also highly resistant to oil, grease, dilute aqueous acids, alkalis and saline solutions, as well as to aliphatic hydrocarbons, such as white spirit, and alcohols.

Special features: VINNOL® H 40/43 TF is a high vinyl acetate containing copolymer. It is therefore especially suitable as a cobinder for formulating flexible VINNOL®-paint and printing ink formulations. It is also highly recommended to reduce the sealing temperature in VINNOL®-based heat sealing lacquers. The solubility in various monomers enables to use VINNOL® H 40/43 TF as an additive in solvent-free 100% systems to improve adhesion and pigment wetting or to reduce shrinking. VINNOL® H 40/43 TF also shows a surprisingly good compatibility with ester soluble nitrocellulose resins and can be used for their modification.

Application: Typical applications for VINNOL® H 40/43 TF:

  • Heat-sealable lacquers
  • Printing inks
  • Paper and film coatings
  • Wood varnishes
  • Strippable lacquers
  • Masonry paints
  • Road-marking paints

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.750 g/ccDIN EN ISO 60
Density 1.33 g/ccDIN 66137-2
Volatiles <= 2.0 %
Particle Size <= 1000 µm
Viscosity 20 - 30 cP20% solids in MEK; DIN 53015
Molecular Weight 40000 - 50000 g/mol
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 58.0 °CDIN 53765/ISO 11357-5
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 35.9 - 37.1 %
 
Descriptive Properties
K-Value41-43DIN EN ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Wacker® TNE 50 Silicone Release Agent
Wacker Wacker® TN Silicone Release Agent
Wacker Wacker® Catalyst OL Release Coating
Wacker Wacker® Catalyst EM 454 Release Coating-Silicone Emulsion
Wacker Wacker® Catalyst EM 440 Release Coating-Silicone Emulsion

PWACK9682 / 205211

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.