MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Alcryn® 2170 BK Melt Processable Rubber
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades bond to polycarbonate, ABS, polycarbonate/ABS alloys, SAN, ASA, copolyester elastomers and TPUs, as well as both flexible and rigid PVC.

Applications:

  • Injection-molded and overmolded parts
  • Soft touch handles and grips
  • Automotive interior applications
  • Seals and gaskets for automotive insert molding
  • Noise and vibration deadening
  • Blow-molded parts
  • Tubing and hose
  • Wire and cable jackets
  • Coated fabrics and sheet goods
  • Window and door weatherstripping
  • Information provided by Advanced Polymer Alloys

    Former product line of Advanced Polymer Alloys (APA), acquired by A. Schulman in 2014.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 1.21 g/ccASTM D471
    Viscosity 275000 cP
    @Shear Rate 300 1/s,
    Temperature 190 °C
    ASTM D3835
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore A 65After 7 days at 125°C; ASTM D573
     69ASTM D2240
    Tensile Strength at Break 1711 psiASTM D412
     2087 psiAfter 7 days at 125°C; ASTM D573
    Elongation at Break 547.2 %After 7 days at 125°C; ASTM D573
     570 %ASTM D412
    100% Modulus 0.435 ksi
    @Strain 100 %
    ASTM D412
     0.6351 ksi
    @Strain 100 %
    After 7 days at 125°C; ASTM D573
    Graves Tear Strength 325.2 pli
    @Temperature 24.0 °C
    Die C; ASTM D624
    Compression Set 19 %
    @Temperature 24.0 °C,
    Time 79200 sec
    ASTM D395
     89 %
    @Temperature 100 °C,
    Time 79200 sec
    ASTM D395
    Tensile Set 15 %ASTM D412
     
    Thermal PropertiesOriginal ValueComments
    Brittleness Temperature -58.0 °CASTM D746
    Clash Berg Stiffness Temperature -38.0 °C69 Mpa; ASTM D1043
     
    Processing PropertiesOriginal ValueComments
    Processing Temperature 177 °C
     
    Descriptive Properties
    Fluid Resistance - Volume Change, % (ASTM D471)-16After 7 Days in ASTM Oil No. 1 At 212°F (100°C)
     17After 7 Days in ASTM Ref. Fuel no. B at 75°F (24°C)
     19After 7 Days in Water at 212°F (100°C)
     6After 7 Days in IRM 903 Oil No. 3 at 212°F (100°C)

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    A. Schulman Alcryn® 2160 BK Melt Processable Rubber
    A. Schulman Alcryn® 1060 BK Melt Processable Rubber
    A. Schulman Alcryn® 2060 NC Melt Processable Rubber
    A. Schulman DuraGrip™ DGR 6060 NC Thermoplastic Elastomer (TPE)
    A. Schulman DuraGrip™ DGR 6160 NC Thermoplastic Elastomer (TPE)

    PAPA013 / 24080

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.