MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
M Chemical GUARD DOG™ UV360 Light Absorber
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GUARD DOG™ UV360 UV absorber is a low volatile dimeric 2-hydroxy benzotriazole based UV absorber which is highly effective in a wide range of polymers and resin compositions.

Applications: Extremely effective in acrylics, alkene polymers, polycarbonates and polyamides. It can be used in combination with phenolic and phosphate antioxidants and HALS to optimize performance in outdoor use.

Performance Benefits:

  • Strong absorption of UV radiation in the 300 - 400 nm range and has a high degree of photostability and excellent thermal properties.
  • Low initial color and low volatility during high processing temperatures and has good extraction resistance. Helpful in preventing plate-out on molds and die-lip build-up

Typical Properties: Free flowing pale yellow powder, Color of 10% Toluene solution: Clear, Solubility@ 20°C (g/100m; solvent): Water <1 mg/L

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/cc
@Temperature 20.0 °C
Volatiles <= 0.50 %
Molecular Weight 658.87 g/mol
Ash <= 0.10 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 194 - 198 °C
 
Optical PropertiesOriginal ValueComments
UV Transmittance >= 97 %
@Thickness 0.450 mm
 >= 98 %
@Thickness 0.500 mm
 
Descriptive Properties
CAS Number103597-45-1
Molecular FormulaC41H50N6O2
Name2- 2'-Methylenebis [6-(2H-benzotriazole-2-yl)-4-(1, 1, 3, 3-tetramethylbutyl) phenol]
Purity (%)99
Recommended Dosage0.15 - 0.60%depending upon the substrate and performance requirements

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
M Chemical GUARD DOG™ UV531 Light Absorber (Flake or Powder), Benzophenone Derivative
M Chemical GUARD DOG™ UV1164 Light Absorber, Triazene Derivative
M Chemical GUARD DOG™ UV234 Light Absorber, Benzotriazole Derivative
MarkeTech Magnesium Oxide (MgO) Single Crystal Substrate
Global EPP PA 6E Extruded Polyamide 6

PMCHEM908 / 135147

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.