MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cotronics Resbond™ 904 Ultra Temp Zirconia Adhesive and Coating
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Ultra Temp 904 is a smooth creamy paste that is easily brushed on ceramics, graphite, metals, etc. to form adhesive bonds and coatings that will withstand 4000°F (2200°C) continuous heat. It has excellent resistance to oxidizing and reducing atmospheres, chemicals and solvents, electricity, molten metals, flame impingement, x-ray radiation, etc.

Applications: bonding, coating, encapsulating, thermocouple protection, high temp. brick facing, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 3000 psi
Compressive Strength 6000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+8 ohm-cm
Dielectric Strength 250 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.10 µin/in-°F
@Temperature 20.0 °C
Thermal Conductivity 10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 4000 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Brandenburger S 5000 Ablation Material for Aeronautics and Space Aviation
AISI Type 304L Stainless Steel
Momentive Performance Materials HPC Boron Nitride (BN)/TiO2 Water Based Coating
ASTM A36 Steel, bar
AK Steel 2205 Duplex Stainless steel

CCOTR0030 / 754

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.