MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: DC 25 is a ZTA Alumina Zirconia Platelet Composite used in dental applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.37 g/ccDIN EN 623-2
Water Absorption 0.00 %Open Porosity; DIN EN 623-2
Particle Size 0.54 µmGrain
Permeability 0.00%, Gas
Weibull Modulus 14DINV ENV 843-5
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 1910HV1; DINV ENV 843-4
Tensile Modulus 357 GPaYoung's; DINV ENV 843-2
Flexural Strength 1350 MPaDIN EN 843-1
 1390 MPaBending Strength; 4-Point; DIN ENV 843-1
Compressive Strength 4700 MPaDIN 51067T1
Poissons Ratio 0.24DINV ENV 843-2
Fracture Toughness 6.40 MPa-m½KIC (SEVNB); DIN CEN/TS 14425-1
Shear Modulus 144 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2000 ohm-cmIEC 672-1
Dielectric Strength 16.5 kV/mmIEC 672-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.10 µm/m-°C
@Temperature 20.0 - 400 °C
DIN EN 821-1
Specific Heat Capacity 0.700 J/g-°CDINV ENV 821-3
Thermal Conductivity 17.0 W/m-KDIN EN 821-2
Maximum Service Temperature, Air 1000 °C
Maximum Service Temperature, Inert 1000 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 74 %DIN EN ISO 12677
Cr2O3 0.30 %DIN EN ISO 12677
Y2O3 0.60 %DIN EN ISO 12677
ZrO2 24 %DIN EN ISO 12677
 
Descriptive Properties
ColorMagenta
Monoclinic Content (%)< 10DIN EN ISO 12677
Other Oxides (%)< 0.1DIN EN ISO 12677
Ra = Arithmetic Mean Roughness Value (µm)<0.06
Radioactivity (Bq/kg)< 25
Thermal Shock Resistance R1 (K)355calculated; R1 = [σs (1-µ)] / (α·E)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
CeramTec ZN 40 Zirconia, ZrO2-MgO
CeramTec B 40 Alumina, 99.1%
CeramTec 771 94% Alumina (Al2O3)

CCERA907 / 107507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.