MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond K6 Ablative Thermal Epoxy Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: TRA-BOND K6 is a three-part, ablative and thermally conductive epoxy compound. This smooth system can be troweled or applied as a potting or coating compound. It is an excellent choice for high temperature protection of electronic parts. It is electrically and thermally insulative. TRA-BOND K6 is impact resistant and dimensionally stable which makes it the choice for lightweight casting requirements for aerospace, ocean and deep space applications. It provides excellent environmental protection.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.670 g/ccMixed
Solids Content 100 %Reactive Solids Content
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 15
Tensile Strength, Yield 100 psi
Elongation at Yield 35 %
Izod Impact, Notched 100 ft-lb/in
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.100 W/m-K
Glass Transition Temp, Tg 24.0 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 4.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 60 min
 
Descriptive Properties
Color Light Brown
Mix Ratio, parts by weight100/75/25Resin/Hardener/Part C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Thermally Conductive
Momentive Performance Materials TSE3280G Thermally Conductive, Heat Cured Silicone Adhesive
CMT Materials HYTAC® W Low Thermal Conductivity Epoxy Syntactic
Momentive Performance Materials TSE3282-G Thermally Conductive Silicone Adhesive
Tra-Con Tra-Bond 2151 Thermally Conductive Electrically Insulating Compound

PTRAC302 / 71230

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.