MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Polycarbonate/PET Polyester Blend
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.12 - 1.47 g/ccAverage value: 1.22 g/cc Grade Count:142
Water Absorption 0.0500 - 0.900 %Average value: 0.234 % Grade Count:51
Moisture Absorption at Equilibrium 0.0200 - 0.700 %Average value: 0.185 % Grade Count:35
Water Absorption at Saturation 0.200 - 0.750 %Average value: 0.439 % Grade Count:9
Viscosity 200 - 600 cP
@Temperature 260 - 270 °C
Average value: 400 cP Grade Count:2
 200 - 600 cP
@Frequency 165 - 1000 Hz
Average value: 400 cP Grade Count:2
Maximum Moisture Content 0.00200 - 0.0200Average value: 0.0182 Grade Count:10
Linear Mold Shrinkage 0.00100 - 0.0180 cm/cmAverage value: 0.00686 cm/cm Grade Count:117
 0.00800 - 0.00800 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00800 cm/cm Grade Count:1
Linear Mold Shrinkage, Transverse 0.00100 - 0.0100 cm/cmAverage value: 0.00601 cm/cm Grade Count:50
 0.00800 - 0.00800 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00800 cm/cm Grade Count:1
Melt Flow 3.00 - 43.0 g/10 minAverage value: 15.8 g/10 min Grade Count:123
Ash 10.0 - 20.0 %Average value: 15.0 % Grade Count:3
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108 - 120Average value: 114 Grade Count:21
Hardness, Shore D 73.0Average value: 73.0 Grade Count:6
Tensile Strength, Ultimate 36.0 - 108 MPaAverage value: 56.4 MPa Grade Count:83
Tensile Strength, Yield 34.0 - 108 MPaAverage value: 54.8 MPa Grade Count:119
Elongation at Break 2.10 - 200 %Average value: 110 % Grade Count:106
Elongation at Yield 2.00 - 86.0 %Average value: 6.76 % Grade Count:62
Modulus of Elasticity 1.16 - 7.65 GPaAverage value: 2.20 GPa Grade Count:65
Flexural Yield Strength 50.0 - 153 MPaAverage value: 83.8 MPa Grade Count:124
Flexural Modulus 1.14 - 7.03 GPaAverage value: 2.25 GPa Grade Count:135
Flexural Strain at Yield 5.00 - 6.20 %Average value: 5.50 % Grade Count:4
Izod Impact 51.0 - 580 JAverage value: 428 J Grade Count:4
Izod Impact, Notched 0.392 - 100 J/cmAverage value: 6.64 J/cm Grade Count:111
 0.0500 - 7.50 J/cm
@Temperature -40.0 - -20.0 °C
Average value: 2.65 J/cm Grade Count:40
 0.490332 - 7.50 J/cm
@Temperature -40.0 - -22.0 °C
Average value: 2.65 J/cm Grade Count:6
 0.490332 - 7.50 J/cm
@Thickness 3.17 - 6.35 mm
Average value: 2.65 J/cm Grade Count:6
Izod Impact, Unnotched 5.58 J/cm - NBAverage value: 6.44 J/cm Grade Count:7
 NB - NB
@Temperature -40.0 - -40.0 °C
Grade Count:2
Izod Impact, Notched (ISO) 1.00 - 75.0 kJ/m²Average value: 21.7 kJ/m² Grade Count:38
 5.00 - 60.0 kJ/m²
@Temperature -40.0 - -10.0 °C
Average value: 15.2 kJ/m² Grade Count:33
Izod Impact, Unnotched (ISO) 38.0 kJ/m² - NBAverage value: 61.5 kJ/m² Grade Count:7
 85.0 kJ/m² - NB
@Temperature -30.0 - -30.0 °C
Average value: 85.0 kJ/m² Grade Count:6
Charpy Impact Unnotched 5.00 J/cm² - NBAverage value: 6.75 J/cm² Grade Count:23
 8.50 J/cm² - NB
@Temperature -30.0 - -30.0 °C
Average value: 8.50 J/cm² Grade Count:14
Charpy Impact, Notched 0.800 - 9.00 J/cm²Average value: 4.40 J/cm² Grade Count:50
 0.600 - 5.00 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 2.44 J/cm² Grade Count:13
Gardner Impact 36.2 - 36.2 JAverage value: 36.2 J Grade Count:12
Dart Drop, Total Energy 5.31 - 95.0 JAverage value: 72.1 J Grade Count:33
 5.13856 - 61.961 J
@Temperature -40.0 - 0.000 °C
Average value: 58.7 J Grade Count:2
 49.0 - 80.2 J
@Temperature -40.0 - 0.000 °C
Average value: 58.7 J Grade Count:3
 49.0 - 80.2 J
@Thickness 3.20 - 3.20 mm
Average value: 58.7 J Grade Count:3
Puncture Energy 36.0 - 55.0 JAverage value: 46.6 J Grade Count:5
 47.0 - 49.0 J
@Temperature -40.0 - -30.0 °C
Average value: 48.3 J Grade Count:4
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 8.00e+9 - 1.00e+18 ohm-cmAverage value: 8.68e+16 ohm-cm Grade Count:32
Surface Resistance 9.00e+9 - 1.00e+17 ohmAverage value: 5.82e+15 ohm Grade Count:24
Static Decay 2.00 secAverage value: 2.00 sec Grade Count:3
Dielectric Constant 3.00 - 4.40Average value: 3.31 Grade Count:10
Dielectric Strength 17.0 - 34.0 kV/mmAverage value: 25.9 kV/mm Grade Count:16
Dissipation Factor 0.00200 - 0.144Average value: 0.0204 Grade Count:10
Arc Resistance 60.0 - 121 secAverage value: 101 sec Grade Count:3
Comparative Tracking Index 100 - 600 VAverage value: 458 V Grade Count:11
 
Thermal PropertiesOriginal ValueComments
CTE, linear 26.0 - 167 µm/m-°CAverage value: 84.1 µm/m-°C Grade Count:60
CTE, linear, Transverse to Flow 45.0 - 140 µm/m-°CAverage value: 85.6 µm/m-°C Grade Count:50
Thermal Conductivity 0.162 - 2.00 W/m-KAverage value: 0.339 W/m-K Grade Count:15
Melting Point 220 - 280 °CAverage value: 247 °C Grade Count:7
Maximum Service Temperature, Air 120 °CAverage value: 120 °C Grade Count:8
Hot Ball Pressure Test 85.0 °CAverage value: 85.0 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 79.0 - 255 °CAverage value: 113 °C Grade Count:84
Deflection Temperature at 1.8 MPa (264 psi) 40.6 - 222 °CAverage value: 98.1 °C Grade Count:125
Vicat Softening Point 90.0 - 204 °CAverage value: 119 °C Grade Count:61
Minimum Service Temperature, Air -40.0 °CAverage value: -40.0 °C Grade Count:8
Glass Transition Temp, Tg 92.0 - 150 °CAverage value: 115 °C Grade Count:5
UL RTI, Electrical 75.0 - 120 °CAverage value: 85.7 °C Grade Count:6
UL RTI, Mechanical with Impact 75.0 - 120 °CAverage value: 83.6 °C Grade Count:6
UL RTI, Mechanical without Impact 75.0 - 120 °CAverage value: 85.7 °C Grade Count:6
Flammability, UL94 HB - 5VAGrade Count:59
Glow Wire Test 750 - 960 °CAverage value: 803 °C Grade Count:11
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.54 - 1.58Average value: 1.55 Grade Count:9
Haze 0.300 - 25.0 %Average value: 3.33 % Grade Count:26
Transmission, Visible 35.0 - 88.0 %Average value: 84.4 % Grade Count:26
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 282 °CAverage value: 200 °C Grade Count:10
Nozzle Temperature 230 - 302 °CAverage value: 259 °C Grade Count:46
Melt Temperature 210 - 330 °CAverage value: 258 °C Grade Count:98
Head Temperature 240 - 270 °CAverage value: 255 °C Grade Count:3
Mold Temperature 18.0 - 110 °CAverage value: 63.7 °C Grade Count:91
Injection Velocity 200 mm/secAverage value: 200 mm/sec Grade Count:6
Drying Temperature 65.0 - 127 °CAverage value: 96.7 °C Grade Count:74
Moisture Content 0.0100 - 0.0200 %Average value: 0.0189 % Grade Count:44
Dew Point -17.8 °CAverage value: -17.8 °C Grade Count:3
Drying Air Flow Rate 22.7 - 28.3 l/minAverage value: 25.5 l/min Grade Count:3
Injection Pressure 4.96 - 172 MPaAverage value: 55.0 MPa Grade Count:9
Vent Depth 0.00130 - 0.0203 cmAverage value: 0.00285 cm Grade Count:32
Cushion 0.635 cmAverage value: 0.635 cm Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Polyram RamShine PVS701 AES, UV Stabilized
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced
Aclo Accucomp ASA ASA001L
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced

O3173a / 89077

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.