MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Tecast Vekton™ 6XAU High Heat Cast Nylon 6 (PA6)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: VEKTON® 6XAU is a high heat weather resistant cast nylon 6 with superior fatigue-resistant and bearing properties.

General Vekton® Cast Nylon Information: VEKTON cast nylon, available in a variety of grades, offers a combination of good mechanical properties, excellent bearing and wear characteristics, and the large-size capabilities of the casting process. Its fatigue resistance, noise damping ability, corrosion resistance, and light weight make VEKTON ideal for metal replacement applications, such as bearings, gears, sheaves, and sprockets. At one-eight the weight of bronze, VEKTON is easier to handle and maintain than metals such as iron, aluminum, brass, and bronze, which it typically replaces in industrial wear applications. Other materials that VEKTON commonly replaces because of its superior performance are laminated phenolics, elastomers, and wood. VEKTON has excellent wear and abrasion resistance, resulting in extended component life and lower maintenance cost. Its formulations are readily available in rod, plate, and tube. Nonstandard shapes, such as rings, discs, and blocks can be economically produced in small quantities with short lead times. Custom parts can be cast-size or near-net-shape with relatively inexpensive tooling.

General Vekton® Application Information: Its unique combination of strength, wear resistance, toughness, machinability, and corrosion resistance make VEKTON cast nylon ideal for bearings, thrust washers, bushings, wear pads, sheaves, rollers, gears, sprockets, and wheels. VEKTON is commonly used in construction equipment, material handling systems, amusement park rides, pulp and paper processing equipment, steel mills and industrial equipment.

Information supplied by Ensinger, Inc.

Key Words: PA6, Polyamide 6
Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.15 - 1.16 g/cc0.0416 - 0.0419 lb/in³ASTM D792
Water Absorption 1.2 %1.2 %at 24 hours; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115ASTM D785
Tensile Strength, Yield 75.8 MPa11000 psiASTM D638
Elongation at Break 20 %20 %ASTM D638
Tensile Modulus 2.41 GPa350 ksiASTM D638
Flexural Strength 86.2 MPa12500 psiASTM D790
Flexural Modulus 2.41 GPa350 ksiASTM D790
Izod Impact, Notched 0.374 J/cm0.700 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Constant  3.7
@Frequency 60 Hz
3.7
@Frequency 60 Hz
ASTM D150
 3.7
@Frequency 60 Hz
3.7
@Frequency 60 Hz
50% RH; ASTM D150
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
Dissipation Factor 0.0020
@Frequency 60 Hz
0.0020
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C
@Temperature 20.0 °C
40.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Melting Point 220 °C428 °FASTM D2133
Maximum Service Temperature, Air 127 °C260 °FLong Term; ASTM UL746B
 177 °C350 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 188 °C370 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C200 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate
Kuraray HYBRAR® Low Rebound Compound # 1
Dow BETADAMP™ 24 Vibration Damper
Donnelly Bros HT 250 High Temperature Mold Grease
Cymat A35620SC 030SS Stabilized Aluminum Foam

PENS57 / 35991

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.